Assessment Of Glass Homogeneity (Portuguese)

A process for sampling glass from a feeder and preperation for polariscopic examination is described. The technique allows the homogeneity to be assessed on the basis of strain at the cord-glass matrix interface.

Author
S B Maia
Origin
Univesidade Federal Do Rio De Janeiro
Journal Title
Vidro November-December 1988 4-8