A bioactive glass series (0.42SiO2−0.10Na2O-0.08CaO-(0.40 − x)ZnO-(x)Ga2O3) was synthesized, and it is efficacy against the Gram (−ve) bacteria Escherichia coli (E. coli), the Gram (+ve) bacteria Staphylococcus aureus (S. aureus), and the fungus Candida albicans (C. albicans), were characterized through liquid broth analysis. The glass series was also seeded in CMC-Dex hydrogels at three different loadings (0.05, 0.10, and 0.25 m2), and the antibacterial and antifungal efficacies of the resulting composites were characterized using both liquid broth and agar diffusion analysis. Liquid broth analysis was conducted using liquid extracts, which for glass samples were obtained after incubation for up to 30 days in both ultrapure water and phosphate buffered saline (PBS), while glass-hydrogel extracts were obtained solely in PBS. Glass extracts (water) decreased C. albicans viability, while those obtained in PBS decreased the viability of both E. coli and C. albicans. Glass-hydrogel extracts exhibited slight inhibition of E. coli and C. albicans. However, none of the liquid extracts decreased S. aureus viability. Glass-hydrogel composites produced inhibition zones in all three microbial cultures, with the greatest efficacy against C. albicans. The results of this study suggest these materials have potential as bone void-filling materials which display antifungal, and possibly, antibacterial properties.

Author
T J Keenan Et Al
Origin
Unknown
Journal Title
J Biomedical Materials Research 105 5 July 2017 1102-1113
Sector
Special Glass
Class
S 4374a

Request article (free for British Glass members)

Antibacterial And Antifungal Properties Of Ga-Bioactive Glass And Ga-Bioactive Glass/Polymeric Hydrogel Composites
J Biomedical Materials Research 105 5 July 2017 1102-1113
S 4374a
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.