The 'Analysis Of Pieces' Method Of Analysing The Causes Of The Spontaneous Breakage Of Toughened Glass Insulators

A quality control method applicable to the production of toughened glass insulators is described.

Author
H Hansheng, M Dingfu, C Guorong
Origin
Nanjing Electro-Ceramic Factory, China
Journal Title
Glass Technology 1991 32 5 177 - 178
Sector
Special Glass
Class
S 581

Request article (free for British Glass members)

The 'Analysis Of Pieces' Method Of Analysing The Causes Of The Spontaneous Breakage Of Toughened Glass Insulators
Glass Technology 1991 32 5 177 - 178
S 581