Advancing Control Of Glass Melters And Forehearths

Advanced control is one of the most important tools for increasing glass quality and production in existing furnaces. Practical experience of advanced control using the GS Expert System II is demonstrated and explained in this paper.

Author
J Chmelar Et Al
Origin
Glass Services Inc, Czech Republic
Journal Title
Glass 77 6 2000 175-176, 178
Sector
Container glass
Class
C 1598

Request article (free for British Glass members)

Advancing Control Of Glass Melters And Forehearths
Glass 77 6 2000 175-176, 178
C 1598
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.