In spite of good thermal efficiency, high energy costs have limited the use of cold-top melting furnaces. In this article the author looks at design advances which make electric melting more economically viable.

Author
R Stormont
Origin
Electroglass Ltd, Uk
Journal Title
Glass 77 1 February 2000 12
Sector
Container glass
Class
C 1503