Advanced Mould Coating Reduces Swabbing Frequency

Although Johnson Radley's Protec GM full-cavity nickel coatig was introduced little more than 18 months ago, it is already being specified for blow and blank moulds by glass container manufactures worldwide.

Author
Un-named
Origin
Unknown
Journal Title
Glass International July/August 2001 8
Sector
Container glass
Class
C 1770

Request article (free for British Glass members)

Advanced Mould Coating Reduces Swabbing Frequency
Glass International July/August 2001 8
C 1770