Stölzle Glass Group wins WorldStar Award for Highland Park - The Dark

Stölzle Glass Group wins WorldStar Award for Highland Park - The Dark

December 12, 2018
Stölzle Flaconnage wins WorldStar Award

Stölzle Flaconnage, the UK site for the global glass manufacturing group, has gained international recognition for its Highland Park – The Dark bottle at the 2018 WorldStar Awards.

The bottle was successful in the beverages category of the awards after the judges were impressed with the design and technical execution of the bottle.

Only 28,000 feeder black whisky bottles were produced featuring prominent Viking runes embossing that harks back to the company’s Orkney base and the island’s Norse and Viking ancestry.

The design was replicated from a bottle dating back to 1876 that showed the Viking symbolism.

Representatives from 20 packaging associations and members of the World Packaging Association decided the WorldStar Award winners in Jinan, China last month, with the companies being revealed last week (December 4).