UK Glass Manufacture - A Mass Balance Study

The glass industry has been taking action for many years to minimise its environmental impact as far as possible. Indeed, improved environmental performance often leads to process improvements and greater efficiencies. This report, published by the Carbon Trust and written by former British Glass employee Andrew Hartley, provided an evidence base for policy decisions concerning the UK’s glass industry. While dated, it still gives useful illustrative data.